MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Silpak RU-480 Liquid Rubber—Urethane RTV
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: RU-480 A/B—80 A Shore is a liquid, two-component, Urethane Elastomer RTV that is easily processed. This system provides a firm, semi-flexible, durable and abrasion resistant rubber compound. Used for a variety of applications including molds, concrete texture stamps and form liners, and rubber parts. Molds are used to cast concrete, wax, and plaster parts. Also makes molds that are compatible for casting Silicone Platinum RTV.

Features:

  • Easy to Process with 2 to 1 Mix Ratio
  • Excellent Strength Properties
  • Dimensionally Stable—Minimal Shrinkage
  • Abrasion resistant for long mold life
Applications: Molds are used to cast concrete, wax, and plaster parts. Also makes molds that are compatible for casting Silicone Platinum RTV. Use for making molds or rubber parts. Molds are used to cast:
  • Making Molds
  • Rubber parts
  • Concrete Texture stamps and form liners

Information provided by Silpak a division of Polytek Development Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/cc
Viscosity 5000 cPInitial Mixed
Storage Temperature 65.0 - 85.0 °F
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80
Tensile Strength 800 psi
Elongation at Break 550 %
Tear Strength 175 pliDie C
 
Processing PropertiesOriginal ValueComments
Cure Time 16.0 hour
@Temperature 22.8 °C
Demold
Shelf Life 6.00 Month
 
Descriptive Properties
ColorYellow/Translucent
Mix Ratio2A:1Bby weight
Pour time20 min
Specific Volume26 in3/lb

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSILPAK008 / 318645

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.