MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
P & P Technology Silicone Sponge
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: The thermal stability of silicone rubber is probably its most important asset. Components made from these rubbers are affected only to a small extent by extremes of temperature, ranging from –90°C to 250°C (depending on grade). Even at temperatures as high as 300°C Silicone rubber will operate for limited periods. Silicone rubber is an excellent electrical insulating material. Resistance to arcing corona, ultra-violet light and ozone is good. It decomposes at 400°C to 500°C leaving an inert, non-flammable and electrically non-conductive residue. It is made of a fine cellular construction composed mainly of non-interconnecting cells and are normally of an off-white color. For continuous use it will stand temperatures between –60°C and -200°C

Information provided by P & P Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 0.0700 - 0.110 MPa
@Strain 40 %
BS4443 Part 1 Method 5B
 0.900 MPa
@Strain 40 %
BS4443 Part 1 Method 5B
Compression Set 5.0 %
@Temperature 150 °C,
Time 252000 sec
recovery period 48 hours 25% compression, after 168 hours at 150°C; BS4443 Part 1 Method 6A
 6.0 %
@Temperature 150 °C,
Time 252000 sec
recovery period 48 hours 25% compression,; BS4443 Part 1 Method 6A
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °CContinuous use
 250 °CComponents made from product
 300 °CLimited periods
Minimum Service Temperature, Air -90.0 °CComponents made from product
 -60.0 °CContinuous use

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain COHRlastic® R10470 Medium General-Purpose Silicone Sponge Rubber
Saint-Gobain COHRlastic® R10480 Soft Low Compression Set Silicone Sponge Rubber
Saint-Gobain COHRlastic® F-12 Silicone Foam
Rogers Corporation Bisco™ RF-120 Cellular Silicone Foam
Rogers Corporation Bisco® MF1 9575 - 75 Silicone, High Performance Foam, Indentation Force Material

PPPTEC025 / 133489

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.