MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK), 30% glass fiber
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Glass Fiber Filled

Material Notes: AvaSpire® AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable grades of reinforced PEEK. These include improved dimensional stability, higher stiffness and lower CLTE from 150°C to 240°C, and lower modulus for greater flexibility at room temperature.

High temperature AV-848 GF30 provides design engineers with an alternative to reinforced PEEK, specifically in demanding applications that require superior toughness, higher structural integrity, and exceptional chemical resistance.

AvaSpire® PAEK can be easily processed using standard thermoplastic melt processing techniques, including injection molding and extrusion.

- Natural: AvaSpire® AV-848 NT

Markets/Uses: Oil & Gas / Down Hole / Back-Up Seal Rings

Applications: Oil/Gas Applications; Seals

Features: Chemical Resistant; Fatigue Resistant; Flame Retardant; Good Dimensional Stability; High Heat Resistance; High Stiffness; High Strength

Injection notes: Back Pressure: Minimum

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.53 g/ccASTM D792
Water Absorption 0.10 %
@Time 86400 sec
ASTM D570
Viscosity 60 cP
@Shear Rate 1000 1/s,
Temperature 400 °C
Melt; ASTM D3835
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
@Thickness 3.18 mm
ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.18 mm
ASTM D955
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 400 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 168 MPa5.0 mm/min; ASTM D638
Elongation at Break 2.3 %5.0 mm/min; ASTM D638
Tensile Modulus 10600 MPa5.0 mm/min; ASTM D638
Flexural Strength 239 MPaASTM D790
Flexural Modulus 9900 MPaASTM D790
Compressive Strength 139 MPaASTM D695
Shear Strength 84.8 MPaASTM D732
Izod Impact, Notched 69.0 J/mASTM D256
Izod Impact, Unnotched 960 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.80e+17 ohm-cmASTM D257
Surface Resistance >= 1.90e+17 ohmASTM D257
Dielectric Constant 3.69
@Frequency 1e+6 Hz
ASTM D150
 3.74
@Frequency 60 Hz
ASTM D150
Dielectric Strength 18.0 kV/mm
@Thickness 3.00 mm
ASTM D149
Dissipation Factor 0.0020
@Frequency 60 Hz
ASTM D150
 0.0060
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.30 J/g-°C
@Temperature 50.0 °C
ASTM C351
 1.70 J/g-°C
@Temperature 200 °C
ASTM C351
Thermal Conductivity 0.290 W/m-KASTM C177
Melting Point 340 °CPeak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 257 °C
@Thickness 3.20 mm
Annealed; ASTM D648
Glass Transition Temp, Tg 158 °CDSC
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 366 °C
Middle Barrel Temperature 371 °C
Front Barrel Temperature 377 °C
Nozzle Temperature 382 °C
Melt Temperature 382 - 404 °CInjection
Mold Temperature 166 - 193 °C
Drying Temperature 149 °C
@Time 14400 sec
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorNatural Color
FormsPellets
Injection RateFast
ProcessingInjection Molding; Machining; Profile Extrusion
Screw Compression Ratio2.0:1.0 to 3.0:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4162 / 279962

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.