MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Solvay Butyl Acid Phosphate
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Identification: Di(n-butyl) phosphoric acid: 45 – 50% and n-Butyl phosphoric acid: 45 – 50%

CAS: 1623-15-0; 107-66-4

Available in: Asia Pacific, Europe, Latin America and North America

Applications: Butyl Acid Phosphate has a variety of industrial uses. It is used as extreme pressure and anti wear additive in lubricant formulation allowing a high Phosphorous content. It is also used as dispersant in a wide range of applications including pigments for ink and paints, as anti-static agent in textile manufacture.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.125 - 1.145 g/ccAV15
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 430 - 500[mg KOH/g]; AV161
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.0020 %AV25
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceClear, Liquid
Color<60Hazen, AV61
CompositionDi Ester48-57%, AV161
 Mono Ester40-48%, AV161

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® 8018HS NC010 PA66-IGF14
Delrin Delrin® 510GR NC000 POM-GF10
Celanese Zytel® 80G14AHS NC010 PA66-IGF14
Esenttia 03H83-AV Homopolymer Polypropylene
A. Schulman PP 1407H-01 Polypropylene High-Impact Polypropylene

WRHOD295 / 137526

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.