MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Orion Performance Compounds i-OnLube™ PA66 GF33 L02 BK Preliminary Data, Nylon 66, MoS2 Filled, 33% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, MoS2 Filled

Material Notes: 21-103-200-001

Description: 33% glass fiber reinforced, MoS2 lubricated nylon 66.

Features:

  • High stiffness
  • High strength
  • Excellent wear resistance
  • Black color
Applications:
  • Automotive
  • Industrial
  • Sporting Goods
Special Instructions: Minimize backpressure to maintain glass fiber integrity.

Information provided by Orion Performance Compounds, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.42 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 17800 psiASTM D638
Tensile Strength, Yield 18000 psiASTM D638
Elongation at Break 1.3 %ASTM D638
Tensile Modulus 1.10e+6 psiASTM D638
Flexural Strength 21000 psiASTM D790
Flexural Modulus 990000 psiASTM D790
Izod Impact, Notched 2.30 ft-lb/inASTM D265
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+12 ohm-cmASTM D257
Surface Resistivity per Square >= 1.00e+12 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 477 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 469 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 540 - 600 °F
Zone 1 530 - 560 °F
Zone 2 540 - 580 °F
Zone 3 540 - 580 °F
Melt Temperature 540 - 600 °F
Mold Temperature 180 - 220 °F
Drying Temperature 170 °F
Dry Time 2.00 - 4.00 hour
Moisture Content 0.020 - 0.060 %
Back Pressure <= 50.0 psi
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PORI9968 / 320659

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.