MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Röchling GLASTHERM S Insulation Sheet
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS

Material Notes: Glastherm Grade S is a general purpose insulation sheet with an economical combination of thermal and physical properties. Not recommended for processes where the continuous operating temperature exceeds 425°F. Grade S is asbestos-free and rugged to withstand rough handling during installation. Suited to rubber molding industry.

Information provided by Glastic Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.84 g/ccASTM D-792
Water Absorption 0.40 %% by wt.; ASTM D-570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 94ASTM D-785
Flexural Strength 18000 psiASTM D-790
Compressive Strength 10000 psi
@Temperature 288 °C
ASTM D-695
 11500 psi
@Temperature 200 °C
ASTM D-695
 16000 psi
@Temperature 150 °C
ASTM D-695
 45000 psi
@Temperature 23.9 °C
ASTM D-695
Compressive Modulus 1.80e+6 psiASTM D-695
Izod Impact, Notched 8.00 ft-lb/inASTM D-256
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 2.00 kV/mmPerpendicular S/T in Air; ASTM D-149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 µm/m-°C
@Temperature 20.0 °C
Across Surface; ASTM D-696
 70.2 µm/m-°C
@Temperature 20.0 °C
Across Thickness; ASTM D-696
Thermal Conductivity 0.260 W/m-KASTM C-177
Maximum Service Temperature, Air 425 °F
Flammability, UL94 HB
@Thickness 23.9 mm
 
Descriptive Properties
Standard ColorTan
Thickness Tolerance in± 0.002

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Uninhibited Naval brass, UNS C46400, H01 (8%) Temper 25 mm rod/bar
Gilding Copper, UNS C21000, Hard Temper
A. Schulman Premi-Glas® 2206-15 CR-SX Fiberglass Reinforced Thermoset SMC
Menzolit Menzolit® SMC 0180 Unsaturated Polyester UP
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 22 wt.% glass

PGLASW5 / 41939

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.