MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper Alloy (CW103C), UNS C17540, TF00 Temper, Forgings
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Precipitation Hardened

Fabrication Properties: Excellent Suitability – Capacity for Being Cold Worked; Good Suitability – Soldering, Brazing, Spot Weld, Seam Weld, Butt Weld, Capacity for Being Hot Formed; Fair Suitability – Gas Shielded Arc Welding, Coated Metal Arc Welding

Typical Uses: Welding and Brazing Components; Plunger tips, die casting

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.318 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 95
Tensile Strength 100 - 140 ksi
 120 ksiTypical
Elongation at Break 10 - 14 %
Tensile Modulus 19600 ksi
Modulus of Rigidity 7538 ksiCalculated
Poissons Ratio 0.30
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000380 ohm-cm45% IACS
Magnetic Permeability 1.0
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.80 µin/in-°F
@Temperature 20.0 - 300 °C
Thermal Conductivity 135 BTU-in/hr-ft²-°F
Melting Point 1880 - 1975 °F
Solidus 1880 °F
Liquidus 1975 °F
 
Component Elements PropertiesOriginal ValueComments
Beryllium, Be 0.40 - 0.70 %
Cobalt, Co 0.80 - 1.3 %
Copper, Cu 96.3 - 98 %As Balance
Iron, Fe <= 0.20 %
Nickel, Ni 0.80 - 1.3 %
Silicon, Si <= 0.20 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC17540x2 / 291607

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.