MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Armacell UT Solaflex Tube and Roll Insulation
Categories: Other Engineering Material

Material Notes: Fiber-free, flexible, closed-cell elastomeric insulation for protection against condensation, mold, energy loss and ultraviolet radiation in high-temperature applications. UT Solaflex is PVC free.
  • 300°F upper temperature limit – ideal for solar applications, hot gas piping and low pressure steam lines
  • Effectively retards degradation due to ultraviolet radiation
  • EPDM-based, closed-cell structure provides excellent condensation and energy loss control
  • Meets 25/50 flame and smoke index ASTM E84

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.20 %
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0400 W/m-KASTM C177 or C518
Maximum Service Temperature, Air 150 °CASTM C534
Minimum Service Temperature, Air -183 °CASTM C534
Flame Spread Index 25ASTM E84
 
Descriptive Properties
Bacterial ResistancePassedASTM G22
Fungi ResistancePassedASTM G21/C1338
Mold GrowthPassedUL181
Smoke Developed Index50ASTM E84
Water Vapor Permeability0.08 perm-inASTM E96, Procedure A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PARMD038 / 186649

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.