MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
3M Dyneon™ FPO 3740 Fluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: 3M™ Dyneon™ FPO 3740 is a peroxide curable fluoroelastomer terpolymer containing 69.5 wt% fluorine. FPO 3740 can be used in compression, transfer or injection molding, and extrusion processes.

Features and Benefits:

  • Improved water, steam, and base resistance when compared to bisphenol cured fluoroelastomers
  • Good press cure physical properties
  • Excellent flow properties

Information provided by the Dyneon division of 3M.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.88 g/cc
Mooney Viscosity 37
@Temperature 121 °C
ML 1+10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75Press cure 10 minutes@ 177°C
 78Post cure 2 hours @ 232°C
Tensile Strength at Break 16.4 MPaPress cure 10 minutes@ 177°C
 22.7 MPaPost cure 2 hours @ 232°C
Elongation at Break 220 %Post cure 2 hours @ 232°C
 230 %Press cure 10 minutes@ 177°C
100% Modulus 0.00480 GPa
@Strain 100 %
Press cure 10 minutes@ 177°C
 0.00630 GPa
@Strain 100 %
Post cure 2 hours @ 232°C
Compression Set 40 %
@Treatment Temp. 200 °C,
Time 252000 sec
ASTM D395 Method B
 
Thermal PropertiesOriginal ValueComments
Transformation Temperature -7.00 °CASTM D1329
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 25 %translucent, but thickness not quantified
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 69.5 %
 
Descriptive Properties
ColorTranslucent
MH, Maximum Toque18.8 inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
ML, Minimum Torque0.9 inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
t2, Time to 2 Inch-lb Rise from Minimum0.4 Minute100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
t'50, Time to 50% Cure0.6 Minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
t'90, Time to 90% Cure1.9 Minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Dyneon™ CCX1029 PTFE, 10% Carbon Fiber Filled

PDYL9976 / 129994

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.