Product Description: An enhanced barrier metalized film with a very broad seal range and can be considered a multipurpose film. This designed of this film allow excellent performance on HFFS machines, especially when laminated with PET. Due to the consistent slip properties, it can be also used in most VFFS applications. In addition to this, the improved barrier properties make it an excellent choice for sensitive product packaging, combining great product protection and yield advantage. Availability: Africa & Middle East, Asia Pacific and Europe Key Features: - Broad sealing range on the inside film
- Good hot tack and very good seal integrity
- Very good moisture and light barrier
- Good oxygen barrier
- Excellent adhesion of aluminum to film
- Easy to convert
- Outstanding metal appearance
- Consistent slip properties
Features: - Flavor & Aroma Barrier
- Gas Barrier
- In Lamination Lap Sealable
- Light Barrier
- Moisture Barrier
- Oxygen Barrier
Applications:- Bakery
- Biscuits/Cookie/Crackers
- Confectionery, Chocolate
- Confectionery, Gum
- Confectionery, Sugar
- Crisps and Snacks
- Frozen Food
- Household and Detergents
- Ice Cream
- Pet Food
Uses:- Box Overwrap Flexible Packaging
- HFFS Flexible Packaging
- Pre-made Bags – Flexible Packaging
- VFFS Flexible Packaging
Processing Method: Cold Seal Adhesive, Inner Web Adhesive Lamination, Solvent Flexographic Printing and Solvent Rotogravure PrintingInformation provided by ExxonMobil |