MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® Care ML67 Medical Grade Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Low viscosity, heat and light stabilized Polyamide 12 for medical application. VESTAMID® Care ML67 is resistant to body fluids and are toxicologically safe.

Features: High bursting strength; Flexible and reliable; High chemical resistance; Low sliding friction; High toughness; Good mechanical properties; Low processing tolerances.

Property data for dry samples.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccISO 1183
Water Absorption 1.4 %Sim. to ISO 62
Moisture Absorption 0.700 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.011 cm/cmISO 294-4, 2577
Melt Flow 60 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 57.0 MPaISO 527
Tensile Strength, Yield 45.0 MPaISO 527
Elongation at Break >= 50 %Nominal; ISO 527
 337 %ISO 527
Elongation at Yield 5.0 %ISO 527
Tensile Modulus 1450 MPaISO 527
50% Modulus 0.0320 GPa
@Strain 50 %
ISO 527
Charpy Impact, Notched 4.00 kJ/m²
@Temperature 23.0 °C
Complete Break; ISO 179/1eA
 5.00 kJ/m²
@Temperature -30.0 °C
Complete Break; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 140 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
Melting Point 178 °CISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 120 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °CISO 75-1/-2
Vicat Softening Point 140 °CMethod B: 10 N, 50 K/h; ISO 306
 170 °CMethod A: 10 N, 50 K/h; ISO 306
Glass Transition Temp, Tg 45.0 °CISO 11357-1/-2
Flammability Test 1.0
@Thickness 1.60 mm
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK826 / 243035

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.