Hostacom PPN 1034 12 is an unfilled PP copolymer with medium melt flow rate and good low temperature impact resistance. The product is also available as a customized color matched, pellet form. This grade is delivered in BLACK color version. Applications: Automotive Parts, Under hoodInformation provided by LyondellBasell. |