MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Copper, UNS C73500
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Excellent corrosion resistance. Fabricated by blanking, drawing, etching, forming and bending, heading and upsetting, roll threading and knurling, shearing, spinning, squeezing, stamping and swaging.

Applications: hollowware, medallion, jewelry, base for silver plate, cosmetic cases, musical instruments, name plates, contacts.

Available as flat products, tube, rod and wire.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.73 g/ccC75200
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 345 - 758 MPa
Tensile Strength, Yield 103 - 579 MPaDepending on temper
Elongation at Break 37 %in 25.4 mm.
Tensile Modulus 18000 ksi
Machinability 20 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000260 ohm-cm6.5% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.90 µin/in-°F
@Temperature 20.0 - 300 °C
Thermal Conductivity 21.0 BTU-in/hr-ft²-°F
Melting Point 1995 - 2075 °F
Solidus 1995 °F
Liquidus 2075 °F
Annealing Point 1000 - 1500 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 72 %
Nickel, Ni 18 %
Zinc, Zn 10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tin-Bearing Copper Nickel, UNS C72500, Quarter Hard flat products
Copper Nickel Tin, UNS C72800
Nickel silver 65-10, UNS C74500
Nickel silver 65-10, UNS C74500, OSO70 Temper flat products
Nickel silver 65-15, UNS C75400, OSO15 Temper sheet or strip

MC73500b1 / 11772

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.