MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik 24.13.LNb Welding wire
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik 24.13.LNb is a niobium stabilized over alloyed filler metal suitable for overlay welding of carbon and low alloy steels, where a type 347 of overlay is required. It is used for gas shielded and submerged arc welding.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 180MIG and TIG
Tensile Strength, Ultimate 600 MPaTIG and MIG
 600 MPaSAW, FLUX 15W
Tensile Strength, Yield 400 MPa
@Strain 0.2 %
TIG and MIG
 400 MPa
@Strain 0.2 %
SAW, FLUX 15W
Elongation at Break 35 %TIG and MIG
 35 %SAW, FLUX 15W
Charpy Impact 90.0 JSAW, FLUX 15W
 110 JTIG and MIG
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 400 °C
Thermal Conductivity 14.0 W/m-K
@Temperature 20.0 °C
 15.0 W/m-K
@Temperature 100 °C
 17.0 W/m-K
@Temperature 300 °C
 18.0 W/m-K
@Temperature 500 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.020 %Filler Metal
 <= 0.020 %MIG
 <= 0.020 %SAW
Chromium, Cr 23.5 %MIG
 23.5 %SAW
 24 %Filler Metal
Manganese, Mn 1.2 %SAW
 2.0 %Filler Metal
 2.0 %MIG
Nickel, Ni 12 %MIG
 12 %SAW
 12.5 %Filler Metal
Niobium, Nb (Columbium, Cb) 0.70 %SAW
 0.75 %MIG
 0.80 %Filler Metal
Phosphorus, P <= 0.020 %Filler Metal
 <= 0.020 %MIG
 <= 0.025 %SAW
Silicon, Si 0.30 %Filler Metal
 0.30 %MIG
 0.30 %SAW
Sulfur, S <= 0.015 %Filler Metal
 <= 0.015 %MIG
 <= 0.015 %SAW

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NSANDV5124 / 199688

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.