MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Asahi Kasei Leona™ TR382 Polyamide 66, Heat Stabilized, Impact
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized

Material Notes: Applications: Automotive parts, electrical & electronic parts, parts for office furnishings.

Information provided by Asahi Kasei Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccDry as Molded; ASTM D792
Density 1.08 g/ccDry as Molded; ISO 1183
Moisture Absorption at Equilibrium 1.7 %
@Temperature 23.0 °C
50% RH; ISO 62
 1.7 %
@Temperature 23.0 °C
50% RH
Linear Mold Shrinkage, Flow 0.017 - 0.025 cm/cmAsahi Kasei
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 89Conditioned at 50% RH; ISO 2039
 107Dry as Molded; ISO 2039
Tensile Strength at Break 45.0 MPaDry as Molded; ISO 527
Tensile Strength 37.0 MPaConditioned at 50% RH; ASTM D638
 54.0 MPaDry as Molded; ASTM D638
Tensile Strength, Yield 35.0 MPaConditioned at 50% RH; ISO 527
 53.0 MPaDry as Molded; ISO 527
Elongation at Break 60 %Dry as Molded; ISO 527
 >= 100 %Conditioned at 50% RH; ISO 527
Elongation at Yield 5.5 %
@Temperature 23.0 °C
Dry as Molded; ISO 527
 28 %
@Temperature 23.0 °C
Conditioned at 50% RH; ISO 527
Tensile Modulus 700 MPaConditioned at 50% RH; ISO 527
 1900 MPaDry as Molded; ISO 527
Flexural Strength 30.0 MPaConditioned at 50% RH; ISO 178
 73.0 MPaDry as Molded; ISO 178
Flexural Modulus 700 MPaConditioned at 50% RH; ISO 178
 2000 MPaDry as Molded; ISO 178
Izod Impact, Notched 1110 J/mDry as Molded; ASTM D256
 1320 J/mConditioned at 50% RH; ASTM D256
Charpy Impact Unnotched NBConditioned at 50% RH; ISO 179
 NBDry as Molded; ISO 179
Charpy Impact, Notched 80.0 kJ/m²Dry as Molded; ISO 179
 NBConditioned at 50% RH; ISO 179
Taber Abrasion, mg/1000 Cycles 6.0Conditioned at 50% RH; ASTM D1044
 
Thermal PropertiesOriginal ValueComments
CTE, linear 110 µm/m-°CDry as Molded; ASTMD 696
Deflection Temperature at 0.46 MPa (66 psi) 183 °CDry as Molded; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °CDry as Molded; ISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Asahi Kasei Leona™ TR161 Polyamide 66, Heat Stabilized, Impact
Arkema Rilsan® BESN BLACK P212 CTL PA11-I-CD
Arkema KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
LyondellBasell Hostacom EKC 133N G31325 Polypropylene Copolymer, 16% Talc Filled
BASF Ultramid® A34 01 PA66 (Dry)

PASAHI8159 / 221186

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.