MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SACO AEI PEXIDAN® R/T Curable Polyethylene Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: PEXIDAN® R/T is a low density XLPE system curable by moisture and consists of a silane pre-grafted base compound A-3001 and a catalyst masterbatch CAT-009. Mixed in the proper proportions (95/5) the two components result in a material that is curable by exposure to 70-95°C hot water or even ambient moisture. PEXIDAN® R/T is listed with the Canadian Standards Association for use in RW-90 and RWU-90 XLPE applications and rated to -40ºC. PEXIDAN® R/T is non-flame-retardant, halogen-free and RoHS-compliant.

Information provided by SACO AEI Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.920 g/ccASTM D792
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Deformation 5.0 %CSA C22.2 No. 38
Storage Temperature <= 30.0 °F
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 2400 psiCSA C22.2 No. 38
 2300 psi
@Temperature 121 °C,
Time 605000 sec
after thermal ageing; ASTM D638
Tensile Strength, Yield 1800 psiCSA C22.2 No. 38
Elongation at Break 400 %CSA C22.2 No. 38
 40 %
@Temperature 150 °C,
Time 900 sec
Hot, Elongation under 0.2 N/mm2 load; SACO AEI DWI-QA-4007 based on ICEA T-28-562
 310 %
@Temperature 121 °C,
Time 605000 sec
after thermal ageing; ASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 7.40e+11 ohm-cm
@Temperature 90.0 °C
After 12 weeks; CSA C22.2 No. 38
 2.83e+12 ohm-cm
@Temperature 15.0 °C
CSA C22.2 No. 38
Dielectric Constant 2.28
@Frequency 1.00e+6 - 1.00e+8 Hz
ASTM D150
 2.38
@Frequency 60.0 Hz
CSA C22.2 No. 38
Dissipation Factor 0.00044
@Frequency 1e+6 Hz
ASTM D150
 0.00046
@Frequency 1e+8 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -75.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Processing Temperature 310 - 340 °Fbarrel zones
Die Temperature 365 °F
Head Temperature 365 °F
 
Descriptive Properties
Degree of Crosslinking72%ASTM D2765

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSACO048 / 249415

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.