Georgia Gulf UV 6685 is a high flow PVC compound designed for thin wall parts and multi-cavity molds. It is ideally suited for a variety of parts requiring resistance to outdoor UV degradation. Information provided by Georgia Gulf Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued. |