MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
LyondellBasell Sequel 2396 SP NH686L Thermoplastic Olefinic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO)

Material Notes: Sequel 2396 SP NH686L thermoplastic polyolefin material is typically used for molded-in-color automotive interior applications that require stiffness, dimensional stability, and high impact characteristics. Applications: Instrument Panels, Interior Automotive Applications

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccASTM D792
Melt Flow 19 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 84ASTM D785
Tensile Strength, Yield 22.0 MPa30mm/min; ASTM D638
Elongation at Break 160 %30mm/min; ASTM D638
Flexural Strength 40.0 MPa30mm/min; ASTM D790
Flexural Modulus 2850 MPa30mm/min; ASTM D790
Izod Impact, Notched 45.0 J/m
@Temperature -30.0 °C
ASTM D 256
 420 J/m
@Temperature 23.0 °C
ASTM D 256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 135 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °CISO 75
 
Descriptive Properties
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Sequel 2396 SP GP BLACK Thermoplastic Olefinic Elastomer
LyondellBasell Sequel 2405 NAT Polyolefin
LyondellBasell Sequel 2396 SP YR400L Thermoplastic Olefinic Elastomer
LyondellBasell Sequel 2396 SP NH767L TRUFFLE GR Thermoplastic Olefinic Elastomer
LyondellBasell Sequel 2396 SP NH690L PREMIUM BLK Thermoplastic Olefinic Elastomer

PEQT8764 / 220398

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.