MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay MIRASHEEN® A-220 Surfactant  (discontinued **)
Categories: Fluid

Material Notes: Description: Liquid, cold pearl additive package that imparts opacity and pearlescence to formulated shampoos, liquid handsoaps, shower gels andrelated products. Requires no heat and readily blends into room temperature formulations.

Identification: Water, Glycol Distearate, Ammonium Laureth Sulfate, Ammonium Lauryl Sulfate, Ammonium Xylene Sulfonate, Cocamide MEA, DMDM Hydantoin.

Available in: Asia Pacific, Europe, Latin America and North America

Applications: MIRASHEEN A-220 is a liquid, cold pearl concentrate that readily disperses into room temperature, liquid formulations to impart an elegant, high luster pearlescent appearance. Typically used at concentrations varying from 1 to 5%, Mirasheen A-220 instantly imparts a high quality pearl to essentially and liquid formulation. For best results it is recommended that Mirasheen A-220 be slowly incorporated into the ambient temperature base formula using smooth, gentle agitation. Once uniform, the final formulation pH and viscosity may be adjusted as desired.

Information provided by Rhodia, Rhodia has been acquired by Solvay. The Mirasheen® brand has been sold to Verdant Specialty Solutions, although this specific grade has been discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/cc
pH 5.0 - 6.010% Aqueous; RP-17601
Viscosity <= 7000 cP
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceWhite, Viscous, Pearly LiquidRP-17620
ColorPearly white
CompositionActive14-16%, MMW=316, RP-17101
 Ammonium Chloride2.5-3.5%, RP-17504
 Anionic Active14-16%, MMW=316, RP-17501
 Total Plate Count<10 cfu/g, RP-17635

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Verdant Specialty Solutions MIRATAINE® CBS Surfactant
Verdant Specialty Solutions MIRANOL® C2M CONC NP Surfactant
Solvay RHODACAL® 60/B Surfactant
Solvay MIRATAINE® H-30 Surfactant
Solvay MIRATAINE® BET CU Surfactant

WRHOD276 / 137507

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.