Masterbatch for the use with SILON Silane crosslinkable PE-Xb Compounds TA 1105 HD, TA 1109 HD and TA 1117 HD. TA 2121 HD contains the cross-linking catalyst to complete together with the above-mentioned graft a Sioplas System. In addition it carries a part of the long term stabilising system for the finished product and a special additive to protect the polymer from degradation caused by metal ions.Information provided by Silon |