MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shanghai Potomer Oxidized Polyethylene Wax
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Property: White powder, lumpy or flakes with flowability. It is a partly oxidized product of polyethylene wax, Since some carboxyl and hydroxyl groups are in molecular chain, its compatibility with polar resins is greatly improved, thus it has excellent internal and external lubrication performance and is soluble in aromatic hydrocarbons.

Applications: OPE is widely used in processing of packing materials and thermoshrink film as external lubricant. It is used as processing auxiliaries for PVC shapes, pipes and plates to increase the surface smoothness of the processed products with an amount of 0.3-0.5%.It can increase the demoulding property effectively and reduce mould-cleaning time significantly in processing plastic products. The product can be also used as new-type lubricating agent with excellent performance for plastics of PVC and polyolefin, etc. It raises lubrication between plastics and metals, improves dispersion of coloring agents and provides products with nice transparency and brightness. It can be used as softening and anti-puncturing agents for textiles. It is also widely used in car wax and leather auxiliaries.

Information provided by Shanghai Potomer International Trade Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Chemical PropertiesOriginal ValueComments
Acid Value 4.0 - 10[KOH mg/g]
 10 - 13[KOH mg/g]
 13 - 16[KOH mg/g]
 
Thermal PropertiesOriginal ValueComments
Softening Point 98.0 - 105 °C
 
Descriptive Properties
Color/Appearancewhite to pale yellow powder or granula

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSPOTOM114 / 284560

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.