MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Greene Tweed Orthetek® RP Polyketone, Random Carbon Fiber
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Greene Tweed offers precision-molded thermoplastic components made form out high-performance Orthtek® composite materials for a variety of demanding medical device applications. Orthtek RP is ideally suited to replace metal due to strength, dimensional stability, low weight and corrosion resistance. Orthtek RP is recommended for noncomplex parts such as nail guides where radiolucentcy and autoclaving are required.

Applications:

  • Medical Trauma – Targeting instruments such as tibial or humeral nail guides
  • Medical Orthopedic – Surgical instruments and retractors

Information provided by Greene Tweed.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.54 g/ccASTM D792
Water Absorption 0.050 %at 212°F (100°C); ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 180000 psiASTM D3039
Elongation at Break 0.50 %ASTM D3039
Tensile Modulus 4.00e+6 psiASTM D3039
Flexural Strength 47000 psiASTM D790
Flexural Modulus 3.70e+6 psiASTM D790
Compressive Strength 37000 psiASTM D695
Compressive Modulus 3.30e+6 psiASTM D695
 
Descriptive Properties
ColorBlack
Fiber OrientationRandom
Fiber Volume, %50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Greene Tweed Orthetek® WF Polyketone, Continuous Woven Carbon Fiber
Greene Tweed WR™ 575 PEEK, Bi-Directional Carbon Fiber Filled
Lotte Advanced Materials Infino® HP-1000XG PC/ABS
RSP Technology RSA-7034 T6 Aluminum Super Alloy
Mitsubishi Chemical Advanced Materials Ketron® 1000 IM Injection Molded Unfilled Polyetheretherketone (ASTM Product Data Sheet)

PGREEN75 / 42369

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.