MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parker Chomerics CHO-BOND® 1030 Conductive Silicone Gasket Adhesive
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Electrically conductive one-component silicone-based RTV adhesive which greatly simplifies the problem of bonding conductive silicone EMI gaskets to metal substrates. This adhesive cures on exposure to moisture in air, contains no acetic acid or other corrosive curing agents, and is workable for up to 30 minutes after exposure to moist air.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 3.50 - 4.00 g/cc
Volatile Organic Compounds (VOC) Content 151 g/l
Thickness 1.18 milRecommended
 
Mechanical PropertiesOriginal ValueComments
Shear Strength >= 200 psiLap
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.050 ohm-cmDC
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 168 hour
@Temperature 23.0 °C
Shelf Life 6.00 Month
 
Descriptive Properties
BinderSilicone
ConsistencyGritty paste
Coverage18.5 cm2 / g
FillerAg/Cu
Mix Ratio1-part
Working Life0.5 hrs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
NeoGraf GRAFOIL® GTC Standard Internal Combustion Graphite, Single Layer Material

PCHOME020 / 28242

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.