Characteristics: Flame retardantSpark resistant Good electrical insulationHeat stability ( 200°C )Good mouldability Low water absorptionLow shrinkageColor-blackSoft/medium flow Applications: Switchgear components exposed to sparkAutomotive ( electrical, electronic ) partsDecor items ( ash trays )Superior quality handles & knobs often exposed to flameAutomotive lamp caps Moudlings exposed to warm & humid climateMoulding exposed to low intensity flame and spark, etc.Information provided by Amity Thermosets Limited |