MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Phosphorus deoxidized Copper high residual phosphorus, UNS C12200
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent hot and cold workability; good forgeability. Fabricated by coining, coppersmithing, drawing and upsetting, hot forging and pressing, spinning, swaging, stamping.

Applications: gas and heater lines, oil burner tubing, plumbing pipe and tubing, condenser, evaporator, heat exchanger, dairy, and distiller tubing, steam and water lines, air, gasoline, and hydraulic lines.

Available as flat products, rod, tube, pipe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.94 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 221 - 379 MPa
Tensile Strength, Yield 69.0 - 345 MPaDepending on temper
Elongation at Break 45 %in 203.2 mm.
Modulus of Elasticity 115 GPaEstimated from similar Cu Alloys
Poissons Ratio 0.31Calculated
Machinability 20 %UNS C36000 (free-cutting brass) = 100%
Forgeability 65 %
Shear Modulus 44.0 GPaEstimated from similar Cu Alloys
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 ohm-cm85% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.80 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0920 BTU/lb-°F
Thermal Conductivity 196 BTU-in/hr-ft²-°F
Melting Point <= 1981 °F
Liquidus 1981 °F
Annealing Point 750 - 1200 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 99.9 %
Phosphorus, P 0.020 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper, UNS C12000
Oxygen-free electronic Copper, UNS C10100
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, H00 Temper flat products
Copper, Cu; Annealed
Oxygen-free high conductivity Copper, Soft, UNS C10200

MC12200b1 / 10590

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.