MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
China-Yixing Longly Refractories Load Bearing Board Corundum-Mullite
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Products with high-purity fused alumina and fused mullite for raw materials, the use of high-tonnage press repression, from ultra-high-temperature sintering; high-purity, the main phase (or corundum mullite) high erosion-resistant, anti-erosion; high-temperature conditions, particularly excellent cross-bending and anti-broken; efficient thermal conductivity and mechanical load power, chemical stability, performance, good thermal shock resistance, excellent creep resistance, long service life; more cost-effective, is the preferred burning kiln furniture for electronic kiln of firing process. Widely used in chemical, ceramics, electronic and magnetic materials of high-temperature furnace.

Application: Magnetic materials, electronic ceramics.

Information Provided by China Yixing Longly Refractories Co. Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 2.80 g/cc
Porosity >= 18 %Apparent
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength >= 29.0 MPahigh temp bending
 >= 110 MPacold bending
Compressive Strength >= 100 MPaAmbient
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air >= 1750 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 >= 86.8 %
Fe2O3 <= 0.080 %
SiO2 <= 9.1 %
 
Descriptive Properties
Refractoriness (°C)>1700Under load temperature, 0.2 MPa, 0.6%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
China-Yixing Longly Refractories Seggar Corundum-Mullite
SUJ 1 High Carbon Bearing Steel (Composition Spec)
China-Yixing Longly Refractories Push Slab Semi-Corundum-Mullite
China-Yixing Longly Refractories Push Slab Corundum-Mullite
China-Yixing Longly Refractories Plate Corundum-Mullite

CYXLR004 / 99306

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.