Nipol 1022 is a copolymer of butadiene and acrylonitrile with medium oil resistance and is directly soluble in many solvents without the necessity of mill breakdown. Sufficient nonstaining antioxidant has been added during manufacture for normal storage conditions. Low viscosity, directly soluble with wide FDA acceptance. |