MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nouryon Ketjenblack EC-600JD powder Carbon black
Categories: Other Engineering Material

Material Notes: Pure electroconductive carbon black with high porosity and specific surface, specifically used for batteries and fuel cells .

CAS number: 1333-86-4

EINECS/ELINCS No: 215-609-9

Applications: Ketjenblack EC-600JD powder is a very pure carbon black extremely suitable for antistatic and electroconductive applications. Due to its unique morphology and the extremely high surface area of approx. 1400 m2/g (BET), only one sixth the amount of Ketjenblack EC-600JD powder is needed compared to conventional electroconductive blacks in order to achieve the same conductivity. The extreme low loading of Ketjenblack EC-600JD powder allows easier processing for those compounds sensitive to filler addition, thus minimizing loss in mechanical and rheological properties. Ketjenblack EC-600JD powder when thoroughly dispersed with the polymer significantly increases the conductivity of the resulting compound.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.0170 - 0.0500 g/cc
Particle Mesh Size 200 Mesh= 98.0 %
 325 Mesh0.8
 
Component Elements PropertiesOriginal ValueComments
H2O, Water >= 1.0 %
 
Descriptive Properties
AppearanceBlack powder
Content440-510 ml/100gPore volume, DBP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY597 / 286120

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.