MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis NAV103 LDPE, post-consumer recycled
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: NAV103 is a mixed-colored low density polyethylene post-consumer recycled (rLDPE) supplied in pellet form for blown film applications. NAV103 is an ideal LDPE used where sustainability and circularity matter. NAV103 is a post-consumer recycled including a large part of recycled post-consumer plastic waste coming from pre-sorted municipal (household) waste. NAV103 is part of the EuCertPlast certificate according to the European Standard EN 15343:2007 (certificate available upon request). Due to the nature of recycleds, some variation in color can be observed between batches. Cas No. 9002-88-4

Typical characteristics:

  • Mixed-colored
  • Filtration: 100 µm
  • Available in homogenized 24-ton truckloads
Applications:
  • Garbage bags
  • Construction films
  • Industrial films

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 g/ccISO 60
Density 0.945 g/ccISO 1183
Melt Flow 0.700 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
Storage Temperature <= 50.0 °C
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 230 %527-3
Film Elongation at Break, TD 410 %527-3
Tensile Modulus 240 MPaMD; ISO 527-3
 265 MPaTD; ISO 527-3
Elmendorf Tear Strength MD 133 gISO 6383-2
Elmendorf Tear Strength TD 561 gISO 6383-2
Dart Drop Test 35.0 gISO 7765-1
Film Tensile Strength at Break, MD 12.0 MPa527-3
Film Tensile Strength at Break, TD 12.0 MPa527-3
 
Processing PropertiesOriginal ValueComments
Melt Temperature 160 - 190 °C
Moisture Content <= 0.0600 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9831 / 323188

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.