System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Covestro Desmopan® 1080AU TPU
Categories:
Polymer
;
Thermoplastic
;
Polyurethane, TP
Material Notes:
Injection molding grade; free from plasticizers; UV stabilized; translucent; Cylindrical pellets; Injection molded engineering parts; hard - soft systems
Mechanical property data for samples at 50% RH.
Information provided by Covestro
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.206
g/cc
ISO 1183-1
Mechanical Properties
Original Value
Comments
Hardness, Shore A
80
ISO 868
Tensile Strength, Ultimate
4570
psi
200 mm/min; DIN 53504
Elongation at Break
723 %
200 mm/min; DIN 53504
Tensile Modulus
24.0
MPa
@Temperature 60.0 °C
storage; ISO 6721-1,-4
34.0
MPa
@Temperature 20.0 °C
storage; ISO 6721-1,-4
171
MPa
@Temperature -20.0 °C
storage; ISO 6721-1,-4
50% Modulus
0.00330
GPa
@Strain 50 %
200 mm/min; DIN 53504
100% Modulus
0.00410
GPa
@Strain 100 %
200 mm/min; DIN 53504
200% Modulus
0.00760
GPa
@Strain 200 %
200 mm/min; DIN 53504
Rebound
44 %
Resilience; ISO 4662
Tear Strength
56.0
kN/m
500 mm/min; ISO 34-1
Abrasion
35
mm3; ISO 4649 method A
Compression Set
22 %
@Temperature 23.0 °C,
Time 259000 sec
ISO 815
31 %
@Temperature 70.0 °C,
Time 86400 sec
DIN ISO 815-1, Method C
41 %
@Temperature 70.0 °C,
Time 86400 sec
ISO 815
Processing Properties
Original Value
Comments
Melt Temperature
185
-
200
°C
Mold Temperature
20.0
°C
Drying Temperature
80.0
°C
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Covestro Desmopan® 1085A TPU
Covestro Desmopan® 453 DPS 041 TPU
Covestro Desmopan® 1092A TPU
Covestro Desmopan® 1045D TPU
Covestro Desmopan® 2786A GMP 045 TPU
PCOVEST0688 / 202471
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.