MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess Addocat® 30EL08 PU Catalyst/Activator
Categories: Other Engineering Material; Catalyst/Initiator

Material Notes: Addocat 30EL08 is a catalyst for the production of polyurethane elastomers by rotational casting. Addocat 30EL08 is used for reactive systems, based on Desmodur® VP.PU 0356. Depending on the hardness of the elastomer 6 - 15 pbw of Addocat 30EL08 should be added per 100 pbw of Desmodur VP.PU 0356. Addocat 30EL08 increases the activity of the casting system and provides adjustment of the flowability for rotational casting, e.g. for the production of roller coverings.

Function: Catalyst for the production of polyurethane elastomers by rotational casting.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/cc
@Temperature 40.0 °C
 1.03 g/cc
@Temperature 20.0 °C
Water Absorption <= 0.15 %
Viscosity >= 1200 cP
@Temperature 40.0 °C
 >= 3850 cP
@Temperature 25.0 °C
 >= 6000 cP
@Temperature 20.0 °C
 
Chemical PropertiesOriginal ValueComments
Acid Value 13 - 17[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Melting Point -15.0 °CFreezing Point
Boiling Point 295 °CInitial
Flash Point 186 °CASTM D93, DIN EN 22719
 
Descriptive Properties
Amine number293-313 mg KOH/g
Hydroxyl value330 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Baybond® PU 406 Polyurethane
Ensinger Hydex™ 301 Rigid Polyurethane (PU)
Ensinger Hydex™ 202 Rigid Polyurethane (PU)
Covestro Baybond® PU 330 Polyester Urethane Polymer
Lanxess Addocat® 102 PU Catalyst/Activator

PLANY8177 / 208570

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.