MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil LDPE LD 185JD Low Density Polyethylene Resin (European Grade)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of lamination films.

Availability: Africa & Middle East and Europe

Additive:

  • Antiblock: 1800 ppm
  • Slip: 330 ppm
  • Thermal Stabilizer: Yes
Applications:
  • Co-Extrusion Films
  • Display Packaging Film
  • Food packaging
  • Form Fill and Seal Packaging
  • High Quality Lamination
  • Lamination Film

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/ccExxonMobil method
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 1800 ppm
Slip Level 330 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1600 psiASTM D882
Film Tensile Strength at Yield, TD 1600 psiASTM D882
Film Elongation at Break, MD 370 %ASTM D882
Film Elongation at Break, TD 550 %ASTM D882
Elmendorf Tear Strength MD 150 gASTM D1922
Elmendorf Tear Strength TD 110 gASTM D1922
Dart Drop Test 80.0 gASTM D1709A
Film Tensile Strength at Break, MD 4200 psiASTM D882
Film Tensile Strength at Break, TD 3300 psiASTM D882
1% Secant Modulus, MD 30000 psiASTM D882
1% Secant Modulus, TD 35000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 230 °FPeak Melting Point; ExxonMobil method
 
Optical PropertiesOriginal ValueComments
Haze 6.3 %ASTM D1003
Gloss 65 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
ExxonMobil LDPE LD 615BA Low Density Polyethylene Resin (European Grade)
Overview of materials for Low Density Polyethylene (LDPE), Molded
LyondellBasell Purell PE 3020K Low Density Polyethylene (LDPE)
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin (European Grade)

PEX99272 / 175508

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.