MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Freudenberg N466 Nitrile Elastomer (NBR)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: General Purpose; Internal Lubricant. Inferior resistance to ozone, sunlight and natural aging; poor resistance to oxygenated solvents. All testing done on AS568-214 size o-rings

This product was formerly sold under the Freudenberg Simrit division; now Freudenberg Sealing Technologies.

Key Words: CHEMIGUM® , HYCAR® , PARACRIL® , PERBUNAN®, KRYNAC®, NYSYSN®
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccASTM D297
 1.24 g/ccASTM D297
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65Original Property; ASTM D2240
 79Air Aging, 70 hours; ASTM D2240
Tensile Strength, Ultimate 12.7 MPaOriginal Property; ASTM D1414
 2162 psiAir Aging, 70 hours; ASTM D1414
Elongation at Break 377 %Original Property; ASTM D1414
 233.74 %Air Aging, 70 hours; ASTM D1414
Compression Set 71 %
@Temperature 125 °C,
Time 252000 sec
ASTM D395 Method B
 71 %
@Temperature 125 °C,
Time 252000 sec
AS 568-214; ASTM D395
 74 %
@Temperature 125 °C,
Time 252000 sec
ASTM D395, Method B
 74 %
@Temperature 125 °C,
Time 252000 sec
AS 568-018; ASTM D395
 79 %
@Temperature 125 °C,
Time 252000 sec
ASTM D395, Method B
 79 %
@Temperature 125 °C,
Time 252000 sec
AS 568-120; ASTM D395
 
Descriptive Properties
Bend (flat)PassAMS 7271H
Corrosion and AdhesionPassAMS-7271H
Dry Neckdown TestPassAMS-7271H
Volume Change (%), ASTM D47110ASTM Reference Fuel A Immersion, 70 hours at 75°F
 -10ASTM Reference Fuel B Immersion, 70 hours at 75°F plus 48 hours at 158°F dry-out
 51ASTM Reference Fuel B Immersion, 70 hours at 75°F
 7ASTM Reference Fuel B Immersion, 70 hours at 75°F plus 48 hours at 158°F dry-out plus ASTM Reference Fuel A Immersion for 5 hours at 75°F
Wet Neckdown TestPassAMS-7271H

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Freudenberg N470 Hydrocarbon Elastomer Nitrile
Freudenberg N442 Nitrile Elastomer (NBR)
Freudenberg N475 Nitrile Elastomer (NBR)
Freudenberg N456 Nitrile Elastomer (NBR)
Freudenberg N431 Nitrile Elastomer (NBR)

PSIMR143 / 79105

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.