MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Chemlon® 66A Nylon 66, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Notes: 66A is general purpose unfilled injection molding grade of nylon 66.

Availability: Europe

Features: General Purpose

Uses: General Purpose

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 - 1.15 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.014 - 0.019 in/in
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 7980 psiISO 527-2
Tensile Modulus 247000 psiISO 527-2
Flexural Strength 2900 psiISO 178
Flexural Modulus 109000 psiISO 178
Izod Impact, Notched (ISO) 4.30 ft-lb/in²ISO 180
Izod Impact, Unnotched (ISO) NBISO 180
Charpy Impact Unnotched NBISO 179
Charpy Impact, Notched NBISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohmIEC 60093
Dielectric Strength 280 V/mil
@Thickness 3.00 mm
IEC 60243-1
Dissipation Factor 0.040
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index >= 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 347 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 140 °FUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 518 - 554 °F
Middle Barrel Temperature 518 - 554 °F
Front Barrel Temperature 518 - 554 °F
Melt Temperature <= 572 °F
Mold Temperature 176 - 194 °F
Drying Temperature 176 °F
Dry Time 2.00 hour
Screw Speed >= 50 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0401 / 236892

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.