MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rogers Corporation R/bak® SF Supported Firm Cushion Mounting Material
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: R/bak® materials are high-density, open cell, polyurethane foams used to build thickness on the cylinder, provide cushioning and absorb vibration in the Flexographic printing process. The use of R/bak cushioning materials results in uniform quality printing over long run conditions. R/bak materials are available in a variety of length and thickness configurations.

R/bak SF and R/bak SS materials have an integrated polyester support layer to ensure dimensional stability and serve as a mounting base.

Information provided by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 20.0 lb/ft³ASTM D3574-95 Test A
Water Absorption 2.0 %AMS 3568
 5.0 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 16ASTM D2240
Hardness, Shore O 24ASTM D2240
Tensile Strength >= 120 psiASTM D3573 Test E
Elongation at Break >= 100 %ASTM D3573 Test E
Compressive Yield Strength 18.0 psi
@Strain 25 %
Tear Strength >= 1.80 kN/mASTM D624, Die C
Compression Set <= 1.3 %
@Temperature 23.0 °C
ASTM D1667
 <= 3.3 %
@Temperature 70.0 °C
ASTM D3574

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carbon-Core CarbonFoam PU 2 R PU
Plutonium, Pu
Rogers Corporation R/bak® U1A Cushion Mounting Material, Unsupported with Single-sided Acrylic Adhesive
Rogers Corporation R/bak® U Unsupported Cushion Mounting Material
Rogers Corporation R/bak® SS Cushion Mounting Materials, Supported Soft

PROGA943 / 138383

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.