Solbrol LB 4 is a Paraben free blend. It is a liquid blend of Benzoic acid, Sorbic acid, Dehydroacetic acid and Caprylyl Glycol in Benzyl alcohol. This is a wide spectrum and mild blend. The product is liquid, which makes it easy to handle. Inhibition of bacteria growth is reached at usage level of 1100 – 2500 ppm.Information provided by Lanxess. |