MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dover Chemical MAYCO BASE 4220 Sulfurized Methyl Ester Low Viscosity, Staining Sulfurized Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Mayco Base 4220 is a sulfurized methyl ester designed to be used in products where low viscosity, excellent base oil (especially highly refined paraffinic) stability, and high wetting characteristics are key. Mayco Base 4220 possesses relatively low odor for such a highly sulfurized additive and the very low viscosity makes blending the additive into base oil an easy task. Mayco Base 4220 can be utilized as a performance booster sump-side, as it will readily mix with the currently used product in the system, if applied at a point of even mild agitation or circulation Some applications in which Mayco Base 4220 may find use are in products designed for gun drilling honing, and heavy duty grinding. Since Mayco Base 4220 contains active sulfur, it should not be used in products destined for applications on the yellow metals (copper, brass, and bronzes).

Information provided by DoverChem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.990 g/cc
@Temperature 15.6 °C
60/60°F
Density 8.25 lb/gal
Saybolt Viscosity at 100°F 650 SUS
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 4.0[meqKOH/g]
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 204 °CCOC
 
Component Elements PropertiesOriginal ValueComments
Sulfur, S 6.0 %Active
 18 %Total
 
Descriptive Properties
AppearanceDark Brown Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDOVER101 / 217720

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.