MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SMAC SMACARCH® 1236S Damping Material
Categories: Other Engineering Material

Material Notes: Specifications - Shock & vibration insulation for:
  • Electronic equipment from high shock inputs
  • Shipping containers, pallets and skids
  • Rack and chassis mounted COTS electronics
Advantages:
  • Large deflections lowering peak energy levels
  • Lower profile when space is at a premium
  • Can be used as stabilizers or base mountings
  • Can be made fail safe with grounding straps

Information provided by SMAC MontBlac Groupe Technologies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 85.0 °C
Minimum Service Temperature, Air -30.0 °C
 
Descriptive Properties
Frequency12-20 Hz
Load100 daN8 mm-Deflection, -3, axial
 100 daN13 mm-Deflection, -2, axial
 100 daN35 mm-Deflection, -1, axial
 104 daN50 mm-Deflection, -1, radial
 120 daN63 mm-Deflection, -1, axial
 125 daN55 mm-Deflection, -2, axial
 145 daN35 mm-Deflection, -2, axial
 150 daN17 mm-Deflection, -3, axial
 150 daN8 mm-Deflection, -4, axial
 150 daN50 mm-Deflection, -2, radial
 155 daN55 mm-Deflection, -3, axial
 165 daN63 mm-Deflection, -2, axial
 180 daN35 mm-Deflection, -3, axial
 195 daN50 mm-Deflection, -3, radial
 210 daN57 mm-Deflection, -4, axial
 215 daN63 mm-Deflection, -3, axial
 225 daN35 mm-Deflection, -4, axial
 250 daN50 mm-Deflection, -4, radial
 350 daN63 mm-Deflection, -4, axial
 50 daN8 mm-Deflection, -1, axial
 50 daN9 mm-Deflection, -3, radial
 50 daN13 mm-Deflection, -2, radial
 50 daN20 mm-Deflection, -1, radial
 75 daN8 mm-Deflection, -4, radial
 95 daN55 mm-Deflection, -1, axial
Materialsspecific formulation for naval applications
Overall size203 x 114 x 127 mm
Transmissibility at resonance<4
Weight2.2 kg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SMAC SMACSONIC® Classic ST Noise and Vibration Damping
SMAC SMACTANE® 60 1114S- N01 Damping Material
SMAC SMACTANE® SP Damping Material
SMAC SMACWRAP® ST Damping Material, 1 mm
SMAC SMACMOUNT® 2112S Damping Material

PZSMAC019 / 146135

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.