MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Covestro Bayhydrol® UV 2282 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Waterborne, UV-curing Polyurethane Dispersion. In the formulation of physically drying, waterborne UV-curing wood and plastic coatings.

Properties / Applications: Bayhydrol® UV 2282 is used in the formulation of High Quality Waterborne UV-curing Wood coatings, that will normally pass the DIN 68 861-1B norm. After the water has evaporated, the coating is physically dry and handable. UV-Curing (10 m/min per 80 W/cm lamp) will result in a very high final quality. The photo initiator demand is low, 1 - 2 % will be enough (by wt., calculated on solid binder). Coatings based on Bayhydrol® UV 2282 will show good adherence to many substrates, including plastics. To further boost adhesion, and to cope with "shadow curing" Bayhydrol® UV 2282 can be dual cured using our Bayhydur® hardeners, VP LS 2336 preferably.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccDIN EN ISO 2811-2
Volatiles 60 - 62 %1g/1h/125°C; DIN EN ISO 3251
pH 7.0 - 8.5DIN ISO 976
 
Descriptive Properties
Appearancemilky, slightly collodial
Flow time< 50s4 mm cup

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOVEST0184 / 201967

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.