MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Evonik Vestamid® D18 Nylon 612 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Unreinforced

Material Notes: Description: medium-viscosity base product

Applications: monofilaments, bristles with high recovery for paint brushes and tooth brushes

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Key Words: PA612, LN, 14-020
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 52.0 MPaISO 527-2/1A
Elongation at Break >= 50 %ISO 527-2/1A
Elongation at Yield 20 %ISO 527-2/1A
Tensile Modulus 1.70 GPaISO 527-2/1A
Charpy Impact Unnotched NB
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 0.900 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 215 °CPeak Temperature; ISO 3146, ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 170 °CWhen conditioned at 180°C for 1 hour; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °CISO 75
 75.0 °CWhen conditioned at 180°C for 1 hour; ISO 75
Vicat Softening Point 180 °C50N; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm
 
Descriptive Properties
Electrolytic CorrosionA1 StepIEC 60426

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik VESTAMID® EX9200 PA 12
Evonik Vestamid® D18 Nylon 612 (Dry as Molded)
Evonik Vestamid® X7166 Flame Retardant Nylon 12
Evonik Vestamid® L2141 Black Nylon 12
Celanese Zytel® 151 NC010 PA612

PHULA02 / 47362

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.