MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC VALOX™ FR 4521 PBT (Europe)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: VALOX 4521 is a 20% glass filled, high flow, flame retardant Polybutylene Terephthalate (PBT) injection moldable grade. It has excellent chemical resistance and a UL94V0@0.75 flame rating and 5VA@2.0mm.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.58 g/ccASTM D792
Density 1.58 g/ccISO 1183
Filler Content 20 %ASTM D229
Water Absorption 0.28 %23°C/sat; ISO 62
Moisture Absorption 0.0900 %23°C / 50% RH; ISO 62
Viscosity 95 cP
@Shear Rate 1500 1/s,
Temperature 260 °C
melt; ISO 11443
Linear Mold Shrinkage, Flow 0.0030 - 0.0070 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.0060 - 0.0090 cm/cmSABIC method
Melt Flow 19 g/10 min
@Load 2.16 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
 26 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ISO 1133
 65 g/10 min
@Load 5.00 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
 90 g/10 min
@Load 5.00 kg,
Temperature 265 °C
ASTM D1238
 95 g/10 min
@Load 5.00 kg,
Temperature 265 °C
cm³/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ISO 2039-2
Ball Indentation Hardness 142 MPaISO 2039-1
Tensile Strength at Break 110 MPa5 mm/min; ISO 527
 110 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 110 MPa5 mm/min; ASTM D638
 110 MPa5 mm/min; ISO 527
Elongation at Break 2.0 %5 mm/min; ASTM D638
 3.0 %5 mm/min; ISO 527
Elongation at Yield 2.0 %5 mm/min; ASTM D638
 2.0 %5 mm/min; ISO 527
Tensile Modulus 7800 MPa5 mm/min; ASTM D638
 8000 MPa1mm/min; ISO 527
Flexural Strength 155 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
 160 MPa2 mm/min; break; ISO 178
Flexural Yield Strength 155 MPa1.3 mm/min, 50 mm span; ASTM D790
 160 MPa2 mm/min; ISO 178
Flexural Modulus 6500 MPa1.3 mm/min, 50 mm span; ASTM D790
 7000 MPa2 mm/min; ISO 178
Flexural Strain at Break 3.0 %2 mm/min; ISO 178
Izod Impact, Notched 70.0 J/mASTM D256
 65.0 J/m
@Temperature -30.0 °C
ASTM D256
 70.0 J/m
@Temperature 0.000 °C
ASTM D256
Izod Impact, Unnotched 530 J/mASTM D4812
 470 J/m
@Temperature -30.0 °C
ASTM D4812
Izod Impact, Notched (ISO) 8.00 kJ/m²80*10*4; ISO 180/1A
 7.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature 0.000 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 35.0 kJ/m²80*10*4; ISO 180/1U
 30.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched 30.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 40.0 kJ/m²ISO 179/2C
 28.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
 30.0 kJ/m²
@Temperature -30.0 °C
ISO 179/2C
Charpy Impact, Notched 5.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 8.00 kJ/m²ISO 179/2C
 5.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 8.00 kJ/m²
@Temperature -30.0 °C
ISO 179/2C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 3.3
@Frequency 50.0 - 60.0 Hz
IEC 60250
 3.4
@Frequency 1e+6 Hz
IEC 60250
 3.4
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 20.0 kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
 25.0 kV/mm
@Thickness 1.60 mm
in oil; ASTM D149
 25.0 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
 37.0 kV/mm
@Thickness 0.800 mm
in oil; IEC 60243-1
 37.0 kV/mm
@Thickness 0.800 mm
in oil; ASTM D149
Dissipation Factor 0.0010
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.015
@Frequency 1e+6 Hz
ASTM D150
 0.015
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance 120 - 180 secASTM D495
Comparative Tracking Index 275 VIEC 60112
 250 - 400 VUL 746A
Hot Wire Ignition, HWI >= 120 secUL 746A
High Amp Arc Ignition, HAI >= 120 arcsUL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
 25.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
 25.0 µm/m-°C
@Temperature 23.0 - 150 °C
ASTM E831
 27.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 74.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 120 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
 130 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
 180 µm/m-°C
@Temperature 23.0 - 150 °C
ASTM E831
Thermal Conductivity 0.270 W/m-KISO 8302
Hot Ball Pressure Test 125 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 220 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 220 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 218 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 205 °C1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
 207 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 205 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 206 °CRate B/50; ASTM D1525
 208 °CRate B/120; ISO 306
 210 °CRate B/50; ISO 306
 218 °CRate A/50; ASTM D1525
 220 °CRate A/50; ISO 306
UL RTI, Electrical 130 °CUL 746B
UL RTI, Mechanical with Impact 130 °CUL 746B
UL RTI, Mechanical without Impact 130 °CUL 746B
Flammability, UL94 V-0
@Thickness 0.750 mm
UL 94
 5VB
@Thickness 1.50 mm
UL 94
 5VA
@Thickness 2.00 mm
UL 94
Oxygen Index 29 %ISO 4589
Glow Wire Test 960 °C
@Thickness 3.20 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 60.0 °CHopper Temperature
Nozzle Temperature 240 - 260 °CInjection Molding
Zone 1 230 - 245 °C
Zone 2 240 - 255 °C
Zone 3 245 - 265 °C
Melt Temperature 250 - 270 °C
Mold Temperature 40.0 - 100 °C
Drying Temperature 110 - 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10332 / 243799

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.