MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Alcast 70FS Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Fused Silica. Hydraulic bond. Alcast 70FS has been specifically developed as a low thermal conductivity aluminium contact grade with excellent resistance to thermal shock and erosion.

Typical applications: Pre-cast launders for aluminium

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 2.17 g/ccdried to 110°C
Grain Size <= 6000 µm
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 80.0 MPa
@Treatment Temp. 1000 °C
Cold Crushing Strength
 80.0 MPa
@Treatment Temp. 815 °C
Cold Crushing Strength
 80.0 MPa
@Treatment Temp. 110 °C
Cold Crushing Strength
 90.0 MPa
@Treatment Temp. 1300 °C
Cold Crushing Strength
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.730 W/m-K
@Temperature 600 °C
Maximum Service Temperature, Air <= 1300 °C
Shrinkage 0.20 %
@Treatment Temp. 815 °C
 0.30 %
@Treatment Temp. 1000 °C
 1.0 %
@Treatment Temp. 1300 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 18 %
BaO 5.0 %
CaO 2.2 %
Fe2O3 0.20 %
K2O+Na2O 0.10 %Na2O + K2O
MgO 0.10 %
SiO2 74 %
TiO2 0.30 %
 
Descriptive Properties
Net Material Required (kg/m³)2020
Water Addition6-7% by weight, 1.5-1.75L per bag, 25 kg bag weight.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR Dixie Clay Filler

CMORF6324 / 203108

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.