MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC SABIC® LDPE 2404EC PE (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: SABIC® LDPE 2404EC is a tubular LDPE grade for extrusion coating. Its special molecular structure gives a good combination of processing and end-performance properties. SABIC® LDPE 2404EC can be used on low and (very) high line speed extrusion coating and lamination processes. Due to its excellent draw down performance and good adhesion, very thin coating layers can be applied on the substrate. Application SABIC® LDPE2404EC is typically used in extrusion coating and lamination applications, such as liquid packaging, imaging, food packaging, release liners and building & construction. It can be used for coatng on paper board, aluminium foil and other substrates. Due its relative high density (compared to SABIC LDPE 2005EC) it has a higher temperature resistance. Properties Mechanical properties determined on compression moulded specimen (2 mm thick) at test speed of 50 mm/min. Film properties have been measured at film of 25 µm, produced on lab scale equipment. Water vapour permeability at 38 °C and 90 % RH per 24 h. Oxygen permeability at 23 °C and 0 % RH per 24 h. This product is not intended for and must not be used in any pharmaceutical/medical applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccASTM D1505
Water Vapor Transmission 20.0 g/m²/dayISO 15106-3
Oxygen Transmission Rate 0.800 cc/m²/dayISO 15105-2
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
Neck In 13.0 cmMeasured on pilot line at 360 m/min, 300 °C, 10 g/m², airgap 300 mm; SABIC method
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 122 J/gDIN 53765
Melting Point 110 °CDIN 53765
Vicat Softening Point 91.0 °CISO 306
 
Descriptive Properties
Minimal coating weight (DD)1.7 g/m²SABIC method; Measured on pilot line at 320 m/min, 300 °C, airgap 300 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10974 / 244441

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.