MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Arkema LOTADER® AX 8900 Terpolymer Ethylene - Acrylic Ester - Glycidyl Methacrylate
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: LOTADER® AX 8900 is a random terpolymer of ethylene, acrylic ester and glycidyl methacrylate, polymerized under high pressure in an autoclave process. Comonomer content is high. Due to its properties (reactivity, softness), LOTADER® AX 8900 is an additive (toughener) of choice in order to improve the impact strength of engineering thermoplastics like PA, Polyesters (PBT, PET), PC/PBT and PC/ABS alloys, PPS. It can also be use as a compatibilizer for Polyesters/Polyolefins blends and as an adhesive for some laminate structures.

Information provided by Arkema Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/cc
@Temperature 23.0 °C
ISO 1183
Methyl Acrylate Content 24 %FTIR (internal)
Melt Index of Compound 6.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 64ASTM D2240
Hardness, Shore D 18ASTM D2240
Tensile Strength at Break 4.00 MPaASTM D638
Elongation at Break 1100 %ASTM D638
Modulus of Elasticity 0.00800 GPaASTM D638
Flexural Modulus <= 30.0 MPaASTM D638
 
Thermal PropertiesOriginal ValueComments
Melting Point 65.0 °CDSC
Vicat Softening Point <= 40.0 °C
@Load 0.999 kg
ASTM D1525
 
Descriptive Properties
Glycidyl Methacrylate Content (%)8FTRI (internal)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema LOTADER® AX 8840 Copolymer Ethylene - Glycidyl Methacrylate
Oceanchem Group Melamine Polyphosphate (MPP)
Arkema LOTADER® TX 8030 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Arkema LOTADER® 3410 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Arkema LOTADER® 8200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride

PARKG193 / 80091

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.