MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Duratherm HTO-FG Heat Transfer Fluid
Categories: Fluid

Material Notes: Duratherm HTO-FG is ideal for a wide range of closed to atmosphere (inertly sealed) applications requiring a food grade rated thermal fluid. Duratherm HTO-FG meets USDA requirements for incidental food contact (H1) and meets the requirements of 21CFR1783570 and is NSF registered. Duratherm HTO-FG’s use of highly refined base stocks ensures excellent thermal stability. Its low volatility also minimizes vapor pressure at elevated temperatures and Duratherm HTO-FG contains antioxidants, metal deactivators and corrosion inhibitors to further enhance the fluid’s longevity and help protect your system. Duratherm HTO-FG is environmentally friendly, non-toxic, non-hazardous and non-reportable. Duratherm HTO-FG poses no ill effect to worker safety. After its long service life Duratherm HTO-FG can easily be disposed of with other waste oils.

Information provided by Duratherm.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 39.4 lb/ft³ASTM D1298
 41.7 lb/ft³ASTM D1298
 50.6 lb/ft³ASTM D1298
 39.4 lb/ft³
@Temperature 315 °C
 43.1 lb/ft³
@Temperature 225 °C
 51.9 lb/ft³
@Temperature 5.00 °C
Viscosity 0.49 cP
@Temperature 315 °C
Dynamic
 0.92 cP
@Temperature 225 °C
Dynamic
 250.63 cP
@Temperature 5.00 °C
Dynamic
Kinematic Viscosity 0.74 cSt
@Temperature 315 °C
 1.26 cSt
@Temperature 225 °C
 6.34 cSt
@Temperature 100 °C
ASTM D445
 39.35 cSt
@Temperature 40.0 °C
ASTM D445
 286.16 cSt
@Temperature 5.00 °C
Molecular Weight 371 g/molAverage
Vapor Pressure 0.000 atm
@Temperature 38.0 °C
ASTM D2879
 0.000 atm
@Temperature 5.00 °C
 0.00780 atm
@Temperature 225 °C
 0.0230 atm
@Temperature 260 °C
ASTM D2879
 0.0960 atm
@Temperature 315 °C
 0.0990 atm
@Temperature 316 °C
ASTM D2879
 
Thermal PropertiesOriginal ValueComments
CTE, linear 1011 µm/m-°C
Specific Heat Capacity 1.788 J/g-°C
@Temperature 5.00 °C
 1.892 J/g-°C
@Temperature 38.0 °C
 2.478 J/g-°C
@Temperature 225 °C
 2.587 J/g-°C
@Temperature 260 °C
 2.76 J/g-°C
@Temperature 315 °C
 2.763 J/g-°C
@Temperature 316 °C
Thermal Conductivity 0.121 W/m-K
@Temperature 316 °C
 0.121 W/m-K
@Temperature 315 °C
 0.124 W/m-K
@Temperature 260 °C
 0.126 W/m-K
@Temperature 225 °C
 0.136 W/m-K
@Temperature 38.0 °C
 0.138 W/m-K
@Temperature 5.00 °C
Distillation Temperature 372 - 455 °C10% to 90% range; ASTM D2887
Maximum Service Temperature, Air 315 °CBulk/Use Temp.
 332 °CFilm Temp.
Pour Point -15.0 °CASTM D97
Flash Point 218 °CASTM D92
Ignition Temperature 360 °CASTM E-659-78
 
Descriptive Properties
AppearanceClear and bright liquid
Fire Point (°C)231ASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDURA677 / 287875

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.