MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ExxonMobil Bicor™ 70 CSR-M OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: Bicor CSR-M is a one-side matte finish, on-side treated, non-heat sealable OPP film designed for cold seal release as the outer web of a lamination. CSR-M is also an excellent matte finish slip film for heat seal laminations. The paper-like appearance of CSR-M provides a differentiated shelf appeal, with a satiny appearance when reverse printed.

Availability: Latin America, North America and South America

Key Features:

  • Excellent ink adhesion on the treated surface
  • Non-migratory slip system for consistent COF
  • Very uniform low-glass surface
  • Excellent release from cold seal surfaces
Applications:
  • Bakery
  • Biscuits/Cookie/Crackers
  • Confectionery, Chocolate
  • Dairy Products
  • Fresh Produce
Uses:
  • HFFS Flexible Packaging
  • VFFS Flexible Packaging
Processing Method: Cold Seal Adhesive, Outer Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing and Water-based Flexographic Printing

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Vapor Transmission 0.510 g/100 in²/day
@Temperature 38.0 °C
90% RH; ExxonMobil Method
Thickness 0.700 milExxonMobil Method
Coating Weight 9.80 lb/reamExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Coefficient of Friction 0.3524 hr, Matte/Matte; ExxonMobil Method
Film Tensile Strength at Break, MD 16000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 30000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 4.0 %
@Temperature 135 °C
ExxonMobil Method
Shrinkage, TD 3.0 %
@Temperature 135 °C
ExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Haze 72 %ExxonMobil Method
Gloss 8.0 %45°, Matte Surface; ExxonMobil Method
 
Descriptive Properties
Wetting Tension0.82 receding cos thetaTreated Surface
Yield44000 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Bicor™ 120 XRG-2 OPP Film
ExxonMobil Bicor™ 21MB777 OPP Film
ExxonMobil Bicor™ 18 LPX-2 OPP Film
ExxonMobil Bicor™ 15MB440 OPP Film
Overview of materials for Polycarbonate/PET Polyester Blend

PEX99457 / 175693

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.