MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Dow 3099 HVIC COMPOUND
Categories: Fluid; Lubricant; Silicone Base

Material Notes: Former Dow Corning product.

Information provided by Dow Corning

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/cc
@Temperature 25.0 °C
Solids Content 100 %
 
Mechanical PropertiesOriginal ValueComments
Penetration P(0), 1/10 mm 260
Penetration P(60), 1/10 mm 270
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.46e+13 ohm-cm
Dielectric Constant 3.86
@Frequency 100000 Hz
 3.88
@Frequency 100 Hz
Dielectric Strength 285 V/mil
Dissipation Factor 0.0066
@Frequency 100000 Hz
 0.0148
@Frequency 100 Hz
Arc Resistance 800 sec
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204 °C
Minimum Service Temperature, Air -40.0 °C
Flash Point >= 121 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 60.0 Month
 
Descriptive Properties
Colorgrey
Water Resistantyes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWCO246 / 105947

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.