MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BASF Ultradur® B 4406 G6 30% Glass Filled PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Description: Is a PBT, flame-retardant injection-molding grades, with 30% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and lighting components.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/ccISO 1183
Moisture Absorption at Equilibrium 0.20 %23°C; 50% RH
Water Absorption at Saturation 0.40 %DIN 53495/1L
Viscosity Test 108 cm³/gViscosity number; ISO 1628
Linear Mold Shrinkage, Flow 0.0020 cm/cmSheet
Linear Mold Shrinkage, Transverse 0.010 cm/cmSheet
Melt Flow 13.2 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 220 MPaISO 2039-1
Tensile Strength, Yield 145 MPa50 mm/min; ISO 527-2
Elongation at Break 2.3 %50mm/min; ISO 527-2
Modulus of Elasticity 11.3 GPaISO 527-2
Charpy Impact Unnotched 60.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²ISO 179/1eA
Dart Drop, Total Energy <= 5.00 JW501 housing; ISO 6603-1
Tensile Creep Modulus, 1000 hours 7500 MPa
@Strain <=0.5 %
ISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmIEC 93
Surface Resistance 1.00e+13 ohmIEC 93
Dielectric Constant 3.9
@Frequency 1e+6 Hz
IEC 250
 3.9
@Frequency 100 Hz
IEC 250
Dielectric Strength 40.0 kV/mmIEC 243/1
Dissipation Factor 0.0020
@Frequency 100 Hz
IEC 250
 0.015
@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 125 VTest solution B; IEC 112
 200 VTest solution A; IEC 112
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.40 J/g-°CIEC 1006
Thermal Conductivity 0.320 W/m-KDIN 52612
Melting Point 220 - 225 °CDSC; ISO 11357-3
Maximum Service Temperature, Air 125 °Cat 50% loss of tensile strength after 20000h; IEC 216-1
 150 °Cat 50% loss of tensile strength after 5000h; IEC 216-1
 210 °C
Deflection Temperature at 0.46 MPa (66 psi) 225 °CISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 205 °CISO 75-2
Flammability, UL94 V-0
@Thickness 0.800 mm
 V-0
@Thickness 1.60 mm
Glow Wire Test 960 °C
@Thickness 3.00 mm
IEC 695
 
Processing PropertiesOriginal ValueComments
Melt Temperature 206 °Cfor shrinkage test
 250 - 275 °CInjection-molding
Mold Temperature 60.0 - 100 °C
 80.0 °Cfor shrinkage test
 
Descriptive Properties
ColorNatural, Colored, Black and Special Colors
Commercial StatusEurope
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultradur® B 4300 G6 30% Glass Filled PBT
BASF Ultradur® B 4406 G6 Q113 30% Glass Filled PBT
BASF Ultradur® B 4406 G4 PBT
Envalior Pocan® B 4235 000000 PBT, 30% Glass Fiber
Shinkong Synthetic Fibers Shinite® D202G30 PBT, 30% Glass Filled, Fire Retardant

PBASG0112 / 131746

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.