MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Synfoam® AD-30 Syntactic Foam
Categories: Polymer; Thermoset

Material Notes: Castable. SynFoam AD s a two component, room temperature curing, castable syntactic designed for casting lightweight complex shapes, where the need for acoustic transparency is a priority. Synfoam AD shows high levels of echo reduction both at ambient pressure and at operating depth. It has been used in the manufacture of sonar domes and sonar windows in submarines. The cast product provides an acoustically transparent housing that surrounds and protects a marine ship’s sophisticated sonar transducer array. SynFoam AD is available as 1, 2, and 5 gallon kits. Each kit contains an A and B side that must be mixed together prior to casting. Cure is achieved within 24 hours and full properties will be realized after 7 days at room temperature. Densities can be customized to the user's specifications. Please consult the appropriate instructions for limitations of depth of cure.

Information provided by Synfoam®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 28.0 - 32.0 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 800 psi
 
Descriptive Properties
Sound Velocity (m/s)1100

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain Meldin® 3000G Bearing
Rogers Arlon MULTICLAD™ HF Halogen-Free Low-Loss Laminate and Prepreg System
Precision Polymer Engineering N80C Nitrile Rubber
Precision Polymer Engineering N70C Nitrile Rubber
Precision Polymer Engineering N60C Nitrile Rubber

PSYNF031 / 192906

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.