MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Stratasys® Rigur Rubber-Like PolyJet 3D Printing Polymer Combination: Primary: AGILUS30 (FLX2040) / AGILUS30 BLACK (FLX9840); Secondary: VERO
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Using two Polyjet printing materials, manufacturers can print prototypes that simulate the appearance and functionality of polypropylene to test form, fit, and function for applications such as snap-fit assemblies, hinges, durable housings, and packaging. Rigur (RGD450) acts as an advanced polypropylene material substitute that offers durability and great surface finishes. Use Rigur in any office-friendly environment to gain reliable performance and stable prototypes. Durus (RGD430) is the original Simulated Polypropylene material that exhibits great impact resilience and an elongation at break of 44%.

Characteristics

  • Opaque
  • Tough
  • Dimensionally stable
Options
  • Rigur is an office-friendly material engineered to deliver reliable performance and impressive, dimensionally stable prototypes.
  • Rigur comes in a bright, true white with PolyJet technology’s signature fine resolution and smooth curves.
Uses
  • Reusable containers and packaging
  • Flexible, snap-fit applications and living hinges
  • Toys, battery cases, laboratory equipment
  • Loudspeakers and automotive component
Advantages
  • Versatility
  • Fine detail
  • Superior toughness
  • Bright white color for sleek prototypes

Information provided by Proto3000

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40.0 - 50.0FLX9740; FLX9840; ASTM D2240
 50.0 - 55.0FLX9750; FLX9850; ASTM D2240
 55.0 - 60.0FLX9760; FLX9860; ASTM D2240
 60.0 - 70.0FLX9770; FLX9870; ASTM D2240
 80.0 - 85.0FLX9785; FLX9885; ASTM D2240
 85.0 - 90.0FLX9795; FLX9895; ASTM D2240
Tensile Strength 3.00 - 4.00 MPaFLX9740; FLX9840; ASTM D412
 3.00 - 4.00 MPaFLX9750; FLX9850; ASTM D412
 3.50 - 4.50 MPaFLX9760; FLX9860; ASTM D412
 4.00 - 6.00 MPaFLX9770; FLX9870; ASTM D412
 6.00 - 10.0 MPaFLX9785; FLX9885; ASTM D412
 10.0 - 14.0 MPaFLX9795; FLX9895; ASTM D412
Elongation at Break 50.0 - 70.0 %FLX9795; FLX9895; ASTM D412
 70.0 - 90.0 %FLX9785; FLX9885; ASTM D412
 120 - 140 %FLX9770; FLX9870; ASTM D412
 150 - 170 %FLX9760; FLX9860; ASTM D412
 170 - 210 %FLX9750; FLX9850; ASTM D412
 190 - 210 %FLX9740; FLX9840; ASTM D412
Tear Strength 5.88 - 7.85 kN/mFLX9740; FLX9840; ASTM D624
 6.86 - 8.83 kN/mFLX9750; FLX9850; ASTM D624
 6.86 - 9.81 kN/mFLX9760; FLX9860; ASTM D624
 11.8 - 13.7 kN/mFLX9770; FLX9870; ASTM D624
 21.6 - 25.5 kN/mFLX9785; FLX9885; ASTM D624
 25.5 - 29.4 kN/mFLX9795; FLX9895; ASTM D624

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPROTO862 / 322875

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.